Standards library for investment casting

The standards most often cited on drawings and orders for investment castings, with their subject and relevance. Summaries are informative; only the standard itself is normative.

Standards reference

DesignationTitle and relevance to investment castingPublisherSubjectStatus
ISO 8062-12007Geometrical product specifications (GPS) — Dimensional and geometrical tolerances for moulded parts — Part 1: Vocabulary
Defines the terms used for casting tolerances, machining allowance and draft.
ISODimensional tolerancesCheck publisher for current edition
ISO/TS 8062-22013Geometrical product specifications (GPS) — Dimensional and geometrical tolerances for moulded parts — Part 2: Rules
Rules for drawing indication and the relationship between casting and final machined drawing.
ISODimensional tolerancesCheck publisher for current edition
ISO 8062-32023Geometrical product specifications (GPS) — Dimensional and geometrical tolerances for moulded parts — Part 3: General dimensional and geometrical tolerances and machining allowances for castings using ± tolerances for indicated dimensions
Core standard for general casting tolerances: DCTG and GCTG grades and required machining allowance grades. Second edition; replaces ISO 8062-3:2007.
ISODimensional tolerancesCurrent edition verified
ISO 8062-4Geometrical product specifications (GPS) — Dimensional and geometrical tolerances for moulded parts — Part 4: Rules and general tolerances for castings using profile tolerancing in a general datum system
Alternative concept: general surface-profile tolerances for castings defined by 3D CAD models.
ISODimensional tolerancesCheck publisher for current edition
BDG P 690 / VDG P 6902010-07Investment castings — Dimensional tolerances, surface condition, machining allowance
German guideline written specifically for investment castings, with accuracy grades D1 to D3; widely referenced on European drawings.
BDG / VDGDimensional tolerancesCurrent edition verified
VDG P 6952008-12Technische Lieferbedingungen für Feingussstücke — Allgemeine Bedingungen
General technical delivery conditions for investment castings.
BDG / VDGDelivery conditionsCurrent edition verified
ISO 2768-11989General tolerances — Part 1: Tolerances for linear and angular dimensions without individual tolerance indications
General tolerances for machined features; not intended as a default for as-cast dimensions.
ISODimensional tolerancesCheck publisher for current edition
ISO 2768-21989General tolerances — Part 2: Geometrical tolerances for features without individual tolerance indications
Still found on many legacy drawings (classes H, K, L).
ISODimensional tolerancesWithdrawn
Withdrawn 2021; replaced by ISO 22081:2021.
ISO 220812021Geometrical product specifications (GPS) — Geometrical tolerancing — General geometrical specifications and general size specifications
Current rules for stating general geometrical and size specifications on drawings.
ISOGeometrical tolerancingCurrent edition verified
ISO 11012017Geometrical product specifications (GPS) — Geometrical tolerancing — Tolerances of form, orientation, location and run-out
Symbols and rules for flatness, straightness, roundness, position, profile and run-out.
ISOGeometrical tolerancingCheck publisher for current edition
ISO 54592024Geometrical product specifications (GPS) — Geometrical tolerancing — Datums and datum systems
Datums, datum systems and datum targets — essential for locating a casting for measurement and machining. Third edition.
ISOGeometrical tolerancingCurrent edition verified
ISO 80152011Geometrical product specifications (GPS) — Fundamentals — Concepts, principles and rules
Fundamental principles, including independency of size and geometry.
ISOGeometrical tolerancingCheck publisher for current edition
ISO 14405-12016Geometrical product specifications (GPS) — Dimensional tolerancing — Part 1: Linear sizes
Defines what a toleranced linear size means and how it is evaluated.
ISOGeometrical tolerancingCheck publisher for current edition
ISO 14405-22018Geometrical product specifications (GPS) — Dimensional tolerancing — Part 2: Dimensions other than linear or angular sizes
Explains why step heights, centre distances and similar dimensions should be controlled by geometrical tolerances.
ISOGeometrical tolerancingCheck publisher for current edition
ISO 21920-1 / -2 / -32021Geometrical product specifications (GPS) — Surface texture: Profile — Part 1: Indication; Part 2: Terms, definitions and parameters; Part 3: Specification operators
Current profile surface-texture series (Ra, Rz); replaces ISO 1302, ISO 4287 and ISO 4288.
ISOSurfaceCheck publisher for current edition
ISO 199592020Steels, nickel alloys and cobalt alloys investment castings — Visual testing of surface quality
Acceptance criteria for visual surface examination of investment castings.
ISOSurfaceCurrent edition verified
ISO 11971Steel and iron castings — Visual testing of surface quality
Visual surface acceptance for steel and iron castings in general.
ISOSurfaceCheck publisher for current edition
ASTM A997Standard Practice for Investment Castings, Surface Acceptance Standards, Visual Examination
Visual acceptance levels for investment casting surfaces.
ASTMSurfaceCheck publisher for current edition
ASTM A802Standard Practice for Steel Castings, Surface Acceptance Standards, Visual Examination
Visual acceptance levels for steel castings using reference comparators.
ASTMSurfaceCheck publisher for current edition
MSS SP-55Quality Standard for Steel Castings for Valves, Flanges, Fittings, and Other Piping Components — Visual Method for Evaluation of Surface Irregularities
Photographic reference standard commonly cited for valve and pump castings.
MSSSurfaceCheck publisher for current edition
ISO 16468Investment castings (steel, nickel alloys and cobalt alloys) — General technical requirements
General technical delivery requirements specific to investment castings.
ISODelivery conditionsCheck publisher for current edition
ISO 4990Steel castings — General technical delivery requirements
Ordering information, test units, re-tests and documentation for steel castings.
ISODelivery conditionsCheck publisher for current edition
EN 1559-1 / -2Founding — Technical conditions of delivery — Part 1: General; Part 2: Additional requirements for steel castings
European technical delivery conditions for castings.
CENDelivery conditionsCheck publisher for current edition
ASTM A957/A957MStandard Specification for Investment Castings, Steel and Alloy, Common Requirements, for General Industrial Use
Common requirements invoked by ASTM material specifications when parts are investment cast.
ASTMDelivery conditionsCheck publisher for current edition
ASTM A985/A985MStandard Specification for Steel Investment Castings General Requirements, for Pressure-Containing Parts
General requirements for pressure-containing steel investment castings.
ASTMDelivery conditionsCheck publisher for current edition
ASTM A732/A732MStandard Specification for Castings, Investment, Carbon and Low Alloy Steel for General Application, and Cobalt Alloy for High Strength at Elevated Temperatures
Investment-cast carbon and low-alloy steel grades.
ASTMMaterialsCheck publisher for current edition
ASTM A216/A216MStandard Specification for Steel Castings, Carbon, Suitable for Fusion Welding, for High-Temperature Service
Grades WCA, WCB, WCC for valves, flanges and fittings.
ASTMMaterialsCheck publisher for current edition
ASTM A217/A217MStandard Specification for Steel Castings, Martensitic Stainless and Alloy, for Pressure-Containing Parts, Suitable for High-Temperature Service
Cr-Mo grades such as WC6 and WC9, and CA15.
ASTMMaterialsCheck publisher for current edition
ASTM A352/A352MStandard Specification for Steel Castings, Ferritic and Martensitic, for Pressure-Containing Parts, Suitable for Low-Temperature Service
Impact-tested grades such as LCB and LCC.
ASTMMaterialsCheck publisher for current edition
ASTM A351/A351MStandard Specification for Castings, Austenitic, for Pressure-Containing Parts
CF3, CF8, CF3M, CF8M and higher-alloyed austenitic grades for pressure parts.
ASTMMaterialsCheck publisher for current edition
ASTM A743/A743MStandard Specification for Castings, Iron-Chromium, Iron-Chromium-Nickel, Corrosion Resistant, for General Application
Corrosion-resistant cast grades for general application, including CA15 and CA6NM.
ASTMMaterialsCheck publisher for current edition
ASTM A744/A744MStandard Specification for Castings, Iron-Chromium-Nickel, Corrosion Resistant, for Severe Service
Corrosion-resistant grades with stricter heat-treatment and weld-repair rules.
ASTMMaterialsCheck publisher for current edition
ASTM A747/A747MStandard Specification for Steel Castings, Stainless, Precipitation Hardening
CB7Cu-1 and CB7Cu-2 (cast 17-4 PH and 15-5 PH types) with H-condition properties.
ASTMMaterialsCheck publisher for current edition
ASTM A890/A890MStandard Specification for Castings, Iron-Chromium-Nickel-Molybdenum Corrosion-Resistant, Duplex (Austenitic/Ferritic) for General Application
Duplex and super duplex cast grades for general application.
ASTMMaterialsCheck publisher for current edition
ASTM A995/A995MStandard Specification for Castings, Austenitic-Ferritic (Duplex) Stainless Steel, for Pressure-Containing Parts
Duplex grades for pressure-containing parts.
ASTMMaterialsCheck publisher for current edition
ASTM A297/A297MStandard Specification for Steel Castings, Iron-Chromium and Iron-Chromium-Nickel, Heat Resistant, for General Application
Heat-resistant H-series grades such as HH and HK.
ASTMMaterialsCheck publisher for current edition
ASTM A494/A494MStandard Specification for Castings, Nickel and Nickel Alloy
Cast nickel, Ni-Cu, Ni-Cr-Fe and Ni-Cr-Mo corrosion-resistant grades.
ASTMMaterialsCheck publisher for current edition
ASTM B367Standard Specification for Titanium and Titanium Alloy Castings
Cast titanium grades including C-2 and C-5 (Ti-6Al-4V).
ASTMMaterialsCheck publisher for current edition
ASTM B618/B618MStandard Specification for Aluminum-Alloy Investment Castings
Aluminium alloys and tempers for investment castings.
ASTMMaterialsCheck publisher for current edition
ASTM F75Standard Specification for Cobalt-28 Chromium-6 Molybdenum Alloy Castings and Casting Alloy for Surgical Implants (UNS R30075)
Co-Cr-Mo casting alloy; the specification is written for implant applications.
ASTMMaterialsCheck publisher for current edition
ASTM B148 / B584Standard Specification for Aluminum-Bronze Sand Castings / Copper Alloy Sand Castings for General Applications
Reference composition and properties for copper casting alloys.
ASTMMaterialsCheck publisher for current edition
EN 10283Corrosion resistant steel castings
European corrosion-resistant cast steel grades, e.g. 1.4308, 1.4408, 1.4470.
CENMaterialsCheck publisher for current edition
EN 10213Steel castings for pressure purposes
European cast steels for pressure equipment, e.g. GP240GH, G17CrMo5-5.
CENMaterialsCheck publisher for current edition
EN 10293Steel castings — Steel castings for general engineering uses
European cast steels for general engineering, including quenched and tempered grades.
CENMaterialsCheck publisher for current edition
EN 10295Heat resistant steel castings
European heat-resistant cast grades, e.g. 1.4837, 1.4848.
CENMaterialsCheck publisher for current edition
EN 1706Aluminium and aluminium alloys — Castings — Chemical composition and mechanical properties
European aluminium casting alloys, e.g. EN AC-42100.
CENMaterialsCheck publisher for current edition
EN 1982Copper and copper alloys — Ingots and castings
European copper casting alloys, e.g. CC333G, CC491K.
CENMaterialsCheck publisher for current edition
ISO 97122021Non-destructive testing — Qualification and certification of NDT personnel
Qualification levels 1 to 3 for NDT personnel.
ISONon-destructive testingCheck publisher for current edition
ISO 3452-12021Non-destructive testing — Penetrant testing — Part 1: General principles
General principles of liquid penetrant testing.
ISONon-destructive testingCheck publisher for current edition
EN 1371-2Founding — Liquid penetrant testing — Part 2: Investment castings
Severity levels for penetrant indications specifically on investment castings.
CENNon-destructive testingCheck publisher for current edition
EN 1369Founding — Magnetic particle testing
Severity levels for magnetic particle indications on ferromagnetic castings.
CENNon-destructive testingCheck publisher for current edition
EN 12681-1Founding — Radiographic testing — Part 1: Film techniques
Radiographic testing techniques for castings.
CENNon-destructive testingCheck publisher for current edition
ASTM E192Standard Reference Radiographs of Investment Steel Castings for Aerospace Applications
Reference radiographs for grading discontinuities in thin-walled investment castings.
ASTMNon-destructive testingCheck publisher for current edition
ASTM E446Standard Reference Radiographs for Steel Castings Up to 2 in. (50.8 mm) in Thickness
Reference radiographs widely used for valve and pump castings.
ASTMNon-destructive testingCheck publisher for current edition
ASTM E165/E165MStandard Practice for Liquid Penetrant Testing for General Industry
Penetrant testing practice referenced by ASTM casting specifications.
ASTMNon-destructive testingCheck publisher for current edition
ASTM E709Standard Guide for Magnetic Particle Testing
Magnetic particle testing guide referenced by ASTM casting specifications.
ASTMNon-destructive testingCheck publisher for current edition
ISO 6892-12019Metallic materials — Tensile testing — Part 1: Method of test at room temperature
Tensile test method: yield strength, tensile strength, elongation.
ISOMechanical testingCheck publisher for current edition
ISO 148-12016Metallic materials — Charpy pendulum impact test — Part 1: Test method
Charpy impact test method.
ISOMechanical testingCheck publisher for current edition
ISO 6506-1 / 6507-1 / 6508-1Metallic materials — Brinell / Vickers / Rockwell hardness test — Part 1: Test method
Hardness test methods used for castings and heat-treatment verification.
ISOMechanical testingCheck publisher for current edition
ASTM A370Standard Test Methods and Definitions for Mechanical Testing of Steel Products
Mechanical testing methods invoked by ASTM steel casting specifications.
ASTMMechanical testingCheck publisher for current edition
ASTM E8/E8MStandard Test Methods for Tension Testing of Metallic Materials
Tension testing for non-ferrous and general metallic materials.
ASTMMechanical testingCheck publisher for current edition
ISO 90012026Quality management systems — Requirements
Quality management system requirements. Sixth edition published September 2026; replaces ISO 9001:2015, with a transition period for existing certificates.
ISOQuality and documentsCurrent edition verified
ISO/IEC 170252017General requirements for the competence of testing and calibration laboratories
Basis for accreditation of testing and calibration laboratories.
ISOQuality and documentsCheck publisher for current edition
EN 102042004Metallic products — Types of inspection documents
Defines inspection documents 2.1, 2.2, 3.1 and 3.2.
CENQuality and documentsCheck publisher for current edition
ISO 104742013Steel and steel products — Inspection documents
International counterpart to EN 10204 for inspection documents.
ISOQuality and documentsCheck publisher for current edition

Status column last reviewed: 2026-11. Official sources: ISO · CEN · DIN Media · BDG / VDG · ASTM · ASME · SAE · JSA (JIS) · MSS

About this list

  • Titles are given as published, in the publication language. Relevance notes are original summaries and do not reproduce the content of the standards.
  • Edition and status. Entries marked as verified were checked against publisher information at the date shown. For the others, and in any case before placing an order, check the current edition with the publisher: standards are revised, amended and withdrawn, and ASTM standards carry a year suffix that changes frequently. European and national adoptions (EN ISO, DIN EN ISO, BS EN ISO, NF EN ISO, NEN-EN-ISO) may carry different dates from the ISO edition.
  • Contractual edition. Unless a dated edition is cited on the drawing or order, agree which edition applies.
  • Scope of the list. The list covers general industrial investment casting. Sector-specific specifications, for example for aerospace, pressure equipment, nuclear or medical applications, apply in addition and are not listed here.

Related: tolerances, international equivalents, documentation.